| Physical Properties | Test Method | Unit | Typical Value | |||
| Density, 23℃ | ASTM D1505 | g/cm³ | 1.12 | |||
| Tensile Strength | ASTM D638 | MPa | 15 | |||
| Elongation at Break | ASTM D638 | % | 200 | |||
| After Oven Aging, 168hrs at 136℃ | ASTM D638 | |||||
| Tensile Strength Retention | % | ≥85 | ||||
| Elongation at Break Retention | % | ≥85 | ||||
| Hot Set Test, 200℃, 0.2MPa, 15min | IEC540 | |||||
| Elongation under Loading | % | 60 | ||||
| Permanent Deformation after Cooling | % | 8 | ||||
| Moisture Content | Karl Fisher | ppm | 500 | |||
| Brittleness Temperature | ASTM D746 | ℃ | -40 | |||
| Electrical Properties | ||||||
| DC Volume Resistivity at | ||||||
| 20℃ | ASTM D991 | Ω.cm | 20 | |||
| 90℃ | Ω.cm | 200 | ||||
1. Temperature Setting of Extruder:
| Zone | 1# | 2# | 3# | 4# | Tube | Head |
| Temp. | 90℃ | 100℃ | 108℃ | 108℃ | 118℃ | 118℃ |
2.It's recommended to use stainless steel wire filter(20×40×20).
3. The above temperature setting are the most typical ones. With different extruder devices, it can be adjusted in terms of the practical situation after extrusion in use, combining with melting pressure and current, in order to achieve the best extrusion result.
4. Dry suggestion: temp. 60℃, 4h.
HJ0901 meets the applicable requirements as below when processed under commercial manufacturing practices and testing procedures.
-AEIC CS 7 and CS 8
-ICEA S-66-524/NEMA WC 7
-IEC 60502
-IEC 60840
-UL 1072
HJ0901 specially designed for the request of super clean and smooth of the surface.
HJ0901 is a cross-linkable semi-conductive conductor and insulation shielding compound for High Voltage cables rated voltage up to 132KV.
HJ0901 is suitable for dry vulcanization processing method at high temperature.
It provides nice extrusion fowability, good performance to prevent scorch and stable volume resistivity.
HJ0901 can withstand low temperature of-50 degrees.