| Physical Properties | Test Method | Unit | Standard | Typical Value | ||||
| Density, 23℃ | ASTM D1505 | g/cm³ | ≤1.2 | 1.12 | ||||
| Tensile Strength | ASTM D638 | Mpa | ≥9 | 10 | ||||
| Elongation at Break | ASTM D638 | % | ≥200 | 220 | ||||
| After Oven Aging, 240hrs at 100℃ | ASTM D638 | |||||||
| Tensile Strength | % | ≥80 | ≥85 | |||||
| Elongation at Break | % | ≥80 | ≥85 | |||||
| Moisture Content | Karl Fisher | ppm | ≤500 | 450 | ||||
| Brittleness Temperature | ASTM D746 | ℃ | ≤-40 | -45 | ||||
| Electrical Properties | ||||||||
| DC Volume Resistivity at | ||||||||
| 20℃ | ASTM D991 | Ω.cm | ≤100 | 10 | ||||
| 90℃ | Ω.cm | ≤1000 | 400 | |||||
1. Temperature Setting of Extruder:
| Zone | 1# | 2# | 3# | 4# | Head | Feeding、Water Cooling、Screw | ||
| Temp. | 140℃ | 150℃ | 155℃ | 160℃ | 165℃ | 65℃ | ||
2.It's recommended to use stainless steel wire filter(20×40×20).
3. The above temperature settings are the most typical ones. With different extruder devices, it can be adjusted in terms of the practical situation after extrusion in use, combining with melting pressure and current, in order to achieve the best extrusion result.
HJ0286 meets the applicable requirements as below when processed using sound extrusion practices and testing procedures.
-AEIC CS 8
-ICEA S-94-649
-IEC 60502
HJ0286 is a thermoplastic non-crosslinked insulation shielding compound for silane crosslinkable overhead cable.
It is applicable for warm water crosslinking method, with fine surface smoothness, good fluidity, and anti-coking extrusion characteristics.